[TheForge] Making power hammers
Steve Smith
[email protected]
Fri Nov 29 22:30:02 2002
I've got a slide mount on my press. I hadn't thought of using it on a
hammer, but it makes sense. Lots faster die changes.
Steve
Dan Scheid wrote:
> Steve my air hammer that is of the Kinyon design . It is tall and thin and
> works just find. I went to a slide for the dies the bolts took to long to
> change them I can change my dies in about 10 sec.
> Dan Scheid
> Flying horse forge
> http://home.earthlink.net/~chevalvolant/flyinghorseforge.html
>
>
>>I think a lot of hammers are made with way too heavy a frame. Sure, the
>>anvil and base need to weigh as much as you have room for. I don't see
>>why the back column has to be such a heavy piece--the work is done by
>>the falling ram's momentum transfer, not by pushing against the frame.
>>The push the frame absorbs is gentler and more spread out.
>>
>>Any thoughts?
>>
>>Steve
>>
>>_______________________________________________
>>http://mailman.qth.net/mailman/listinfo/theforge
>>theforge mail list group photo site is
>>http://www.photoaccess.com
>>Login: [email protected]
>>password: anvil
>>___________
>>
>>
>>
>
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>