[TheForge] erasable marker boards

Bruce Freeman [email protected]
Mon Nov 25 14:22:00 2002


Maybe, but I doubt it.  These boards are some sort of plastic.  If your =
paint matches the characteristics of that plastic, then you're home free.  =
Fail to do that and even the "erasable" markers may permanently mark the =
stuff.  I consider these boards to be a pain in the a** because you can =
ONLY use special markers on them, and sometimes those won't erase off =
easily.

Depending upon your application, I have a possibly better idea.  Paint the =
back of a sheet of glass with white paint (whatever sticks).  Then use any =
sort of glass-marking (i.e., most any) marker on the opposite side from =
the paint.  To erase, use 91% isopropyl alcohol (available in drug =
stores). =20

Bruce=20
NJ

>>> [email protected] 11/25/02 12:00PM >>>
All,

I know that they have the black paint for chalk boards.  What I'm =
wondering=20
is if they have a special paint for the white erasable marker boards.

Know anything about this?  Will any good white high gloss enamel work?

Dave Brown