[TheForge] Fireclay lining

[email protected] [email protected]
Sun Nov 24 00:27:00 2002


To All,
I purchased a small rivet forge several years ago and it says right in the 
casting to line it with fireclay.  Fireclay is available from most any 
masonary supply center and should be mixed 1/3 clay, 1/3 portland cement and 
1/3 sand or so says one opinion that was given to me.  I just have not had 
the time to try it.  I probably going to go with 1/3 clay and 2/3 "sacrete" 
for my first shot at it.
By the way mine is cracked probably from it not being lined at some point in 
time.

hochewa

In a message dated 11/23/02 6:06:11 PM Eastern Standard Time, 
[email protected] writes:

<< That's why it's cast iron, you don't need clay. Heat goes up.
 dan tull
 georgia
 abba, afc, S.C. psba, obg,sofa
 ----- Original Message -----
 From: "TOOL GYPSY" <[email protected]>
 To: <[email protected]>
 Sent: Saturday, November 23, 2002 10:30 AM
 Subject: [TheForge] Fireclay lining
 
 
 > Hello
 >    I just got a small forge ,its heavy cast iron.My question is Do i have
 to
 > line it with clay as it doesnt seem to have any remnants of past clay?
 >                                    Regards
 >                                       Pat
 > >>