The sheet size is a simple matter of how big you build the table, mine is
1200 x 1200, I will send a pic as soon as I figure out my USB problems so I
can get it off my camera, (just reinstalled windows). Have a good dig around
the torchmate site, he has a lot of great info on there, even has a great 3d
model you can download of the construction of the table and view in most cad
programs. Any questions Id be glad to share what Ive learned.
----- Original Message -----
From: "Ralph Sproul" <[email protected]>
To: <[email protected]>
Sent: 19 November, 2002 4:01 AM
Subject: Re: [TheForge] Cnc Plasma cutting table
> Shannell, You've sparked an interest in seeing this unit you've
> made, any chance you could post a picture or send me one of this unit?
How
> large a sheet does it take? a 48" x 48" or full sheet? or smaller
sections?
>
> Ralph
>
>
> ----- Original Message -----
> From: "Shannell Sugrue" <[email protected]>
> To: <[email protected]>
> Sent: Tuesday, November 19, 2002 1:53 PM
> Subject: Re: [TheForge] Cnc Plasma cutting table
>
>
> > Build your own, they will sell you the electronics at inflated prices
> (IMO),
> > you can buy 3 axis drivers for 1-300 bucks US and the rest is simple
> > engineering, copy their designs for the table they are basic and work
> well,
> > get a torch without high frequency start, you dont even need a machine
> > torch, you can usually retro fit machine switching of the torch to the
> > machine easily. I built mine for about $700 USD excluding plasma of
> course,
> > if the electrics scare you its just basic wiring up of the different
> > components. There are a lot of web resources out there for cnc.
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: [email protected]
> > password: anvil
> > ___________
> >
> >
> >
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>