If your son wants to do forging but the school frowns on a forge fire,
why not use either modeling clay and wooden tools or bar solder and
light hammers. Use a piece of RR rail for an anvil. With some practice,
your son should be able to make things that he would otherwise make in
steel.
Mark Williams
Snow Hill, Maryland
----- Original Message -----
From: "Kelloughs" <[email protected]>
To: <[email protected]>
Sent: Tuesday, November 05, 2002 3:41 PM
Subject: [TheForge] Science fair project
> My 10 year old son is going to do a science fair project soon. He
frequently helps me at the forge and also likes to do his own little
jobs. I
thought that it would be a good idea to do his project on blacksmithing
as
no one at his school has done a project on this subject in recent past
(that
we know about).
> My question would be: does any one know of a good project for him, or
any
recourses we could use? Please keep in mind that he is ten years old,
and I
want him to pretty much do the job him self with only my supervision.
> Thanks in advance
> John Kellough
>
> --- StripMime Report -- processed MIME parts ---
> multipart/alternative
> text/plain (text body -- kept)
> text/html
> The reason this message is shown is because the post was in HTML
> or had an attachment. Attachments are not allowed.
> Please post in Plain-Text only.---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: [email protected]
password: anvil
___________