Rob, Ralph, Mike, Phlip, and anyone else with suggestions,
I've posted a picture in the "anything else" folder on Photo Access.
It's a sketch on my idea of the corner hook detail for the Fire Grid.
Each corner angle would lap and be riveted. The vertical portion of
each angle would be drawn out and form the hook(actually two hooks side
by side) Best I could determine from the sketches and photo I saw.
Does this look right to you?
For the chain links between the grid and the top plate. Some appear to
be hooks others welded eyes. Should there be a mix or do you think they
were all welded eyes originally? Also lengths of individual links
appear random. Your thoughts?
Rob, I plan to work on this tomorrow and will let you know by days end
if I think there's a chance I can complete it in time to ship to you.
What's your absolute drop dead date to receive it? I think I have
enough wrought iron to make it but might have to use some pure iron. If
I complete it should I mark it in any way or did you come up with a
theforge mastermyr touch mark to mark all the pieces?
Bill Clemens
Hound and Hare Forge
Ralph wrote:
> I hope this helps.
>
> Frame about 50 X 50 cm: strip width 0.45 cm, thickness 0.25 cm; grid
> rods 49.0 X 1.2 X 0.3-0.5 cm.
> Chain links about 0.6-0.7 cm, total length of each chain about 42 cm.
> Swivel: four-armed plate
> about 16 X 9 cm, thickness 0.3 cm; hook 10.3 X 1.5 X 0.7 cm; the open
> part of the hook maximum
> width 1.5 cm.
>
> Ralph
>
> I do not have a drop dead date. <smile> Tho Rob Fertner does. He is
> the collection point for all the stuff as he will carry it to
> LaCrosse. Unless you are going as well then you can give it to him
> then. But Rob is wanting to have it first part of June.
>
> Ralph
>
>
>
>
> "Good is the enemy of Excellent. Talent is not necessary for Excellence.
> Persistence is necessary for Excellence. And Persistence is a Decision."
>
>
> --- StripMime Report -- processed MIME parts ---
> multipart/mixed
> text/plain (text body -- kept)
> image/jpeg
> The reason this message is shown is because the post was in HTML
> or had an attachment. Attachments are not allowed.
> Please post in Plain-Text only.---
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>
>