[TheForge] Mastermyr

Ralph [email protected]
Sat May 25 00:45:01 2002


I hope this helps.

Frame about 50 X 50 cm: strip width 0.45 cm, thickness 0.25 cm; grid rods 
49.0 X 1.2 X 0.3-0.5 cm.
Chain links about 0.6-0.7 cm, total length of each chain about 42 cm. 
Swivel: four-armed plate
about 16 X 9 cm, thickness 0.3 cm; hook 10.3 X 1.5 X 0.7 cm; the open part 
of the hook maximum
width 1.5 cm.

Ralph

I do not have a drop dead date. <smile> Tho Rob Fertner does. He is the 
collection point for all the stuff as he will carry it to LaCrosse. Unless 
you are going as well then you can give it to him then. But Rob is wanting 
to have it first part of June.

Ralph




"Good is the enemy of Excellent. Talent is not necessary for Excellence.
Persistence is necessary for Excellence. And Persistence is a Decision."


--- StripMime Report -- processed MIME parts ---
multipart/mixed
  text/plain (text body -- kept)
  image/jpeg
The reason this message is shown is because the post was in HTML
or had an attachment. Attachments are not allowed.
Please post in Plain-Text only.---