[TheForge] hard faced dies

[email protected] [email protected]
Thu May 9 09:20:01 2002


thanks pete, that will be my first try. hey did you ever get that big grinder going?  bob.


>At 05:15 AM 5/2/02, you wrote:
>>Bob; Both Bill Epps and of course, Rob Gunther say that superquenched A36 
>>makes satisfactory hammer dies if one works hot...Pete
>>would it work to weld a hard face on A36 to make air hammer dies? if so 
>>any rod recommendations. if not why?
>>
>>thanks.
>>
>>bob