Jeffrey L Jones wrote:
>
> "You will have good results with 2 pair of offset compound leverage
> snips, get left and right hand. The cutting edge is below the mass of
> the tool and you have excellent control. over cut a bit if the
> complexity requires it to allow finishing with a fine file and
> sandpaper."
> Stephen McGehee
>
> Stephen,
> These offset compound leverage snips, will they cut at least 16 gauge
> copper and not distort the cut edge? As my reply to Mike Graf indicates
> I did not make it clear if I was talking ounces or gauges. I am talking
> gauges just because I am familiar with thickness rather than mass. Just
> the center of this door will have 4 copper triangles cut and mated to
> form a diamond. All the cuts must meet exactly with no distortion in the
> copper.
The snips will always give some distortion because they
work by shearing. The only way around this is to cut the
material larger than you need and file to a line. That
will almost certainly prove painfully time consuming.
Plasma arc.