 I think they use STP. :)  Orange degreaser is non toxic. We use some stuff that is 97%  Try something high in citric acid. Like powdered lemonaide mix.  Ammonia would probably work, but who lokes eggs al ammonia.
  phlip_u <[email protected]> wrote: 


Hey, guys- anybody know what this stuff is? I've never run into it 
before. My tendency would be to tell him to heat it, then wire brush 
while hot.....

Phlip

--- In spca-wascaerfrig@y..., PBLoomis@a... wrote:

We recently bought, at Sam's in Gulfport, a set of cast iron 
cookware:
two skillets, a griddle, and a dutch oven with a proper lid but no 
legs, each
with a separate zipper bag, all packed in a reasonably sturdy carry 
box w/
rope handles. Marketed by Wenzel but made in China.
Aye, there's the rub. And rub. And rub.
Our instructions from Lodge Cast Iron say remove the shipping-and-
storage coating before seasoning cast iron cookware. With Lodge ware, 
this is easy. With this Chinese stuff, not so easy. Scrub and scrub,
following the Lodge instructions. Dry it off and more of the stuff 
comes 
off on the paper towel. Scrub and scrub again, with Dawn which will 
eat
through aluminum pans if left alone. Dry it off and more of the stuff 
comes 
off on the paper towel. 
Has anybody else gone thru this?
Does anybody else know what the Chinese used? 
And how to remove it?
If the Chinese used stove blacking, is it poisonous?

Suggestions gratefully received,
Scotti
Knowledge is never wasted, nor is the time to acquire it.
--- End forwarded message ---


_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: [email protected]
password: anvil
___________




---------------------------------
Do You Yahoo!?
Yahoo! Movies - coverage of the 74th Academy Awards�

--- StripMime Report -- processed MIME parts ---
multipart/alternative
  text/plain (text body -- kept)
  text/html
---