Unless you don't mind the expense (or have an excellent source of scrap!), I
would call H13 a waste for power hammer dies. I have a hard time seeing hammer
dies worked so steadily that they start showing oxide colors, at least on the
size of material that fits in my equipment. There is enough mass of metal that
they should stay pretty cool.

Steve Smith

Shannell wrote:

> Sounds like Im going to like this stuff, good for power hammer dies too Id
> guess, how hard is it to anneal, overnight in ashes enough?? What are the
> bad points?
>
> ----- Original Message -----
> From: "Dave Brown" <[email protected]>
> To: <[email protected]>
> Sent: Monday, March 25, 2002 10:42 PM
> Subject: Re: [TheForge] h13 for chisels
>
> > At 05:01 03/25/02 -0500, you wrote:
> >
> > >Any suggustions as to where to purchase H13, and what sizes and quanity
> is it
> > >available in. Thanks, Ralph
> > >
> > >Ralph Neumeister
> >
> > Ralph,
> >
> > Centaur Forge sells short pieces.  They have H13 in 1/2" and 5/8" rounds
> in
> > 8", 10" & 12" pieces.  Prices range from $5 to $7 ea.  I'm told that it
> > comes in an annealed state and you can cut it through with a hack saw ...
> > you won't do this once you harden it.
> >
> > A good scrounge source (generally for 3/8" up to 1/2", maybe more) is
> > injection molding shops and factories.  They use it for ejection
> > pins.  They buy standard lengths with nice flat heads on them.  When one
> in
> > use gets even the slightest bit worn they pull them and put new ones in
> > after cutting to length for the particular mold.  They throw the cut off
> > ends and the old used pins in the dumpster.  There's one member of UMBA
> > that lives near such a plant and they actually save all their reject pins
> > and cut offs for him.  At our last informal gathering here in Green Bay he
> > brought a box full of H13 and we were free to take all we wanted.  Great
> guy.
> >
> > Dave Brown
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login:  [email protected]
> > password:  anvil
> > ___________
> >
> >
> >
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________