This stuff sounds like just the ticket to put in my vise. Now, where do
you get it in nice small pieces?
Dave
At 07:58 03/25/02 -0500, you wrote:
> >
> > What's UHMDP?
>
>Ultra-High Molecular Density Polyethylene, IIRC. A little denser than the
>translucent white stuff they use to make milk jugs.
>
>Sometimes it's called Ultra-High Molecular Weight Polyethylene.
>
>Plastic; tough, heavy, strong, relatively soft-surfaced plastic.
>
>Used to use it for spacers in rebuilding old overhead crane gearboxes.
>Stuff'll stand up to just about anything but heat.