[TheForge] Stone Mason chisels
Dave Brown
[email protected]
Mon Mar 18 15:12:00 2002
Bob,
These are not pavers. These are hand held chisels that one hits with a
hammer. Used for facing, smoothing, chipping, etc.... Not just for
busting up stuff. But I suppose some 1045 for a test piece wouldn't hurt.
Dave
At 13:54 03/18/02 -0600, you wrote:
>dave,
>
>the pavement breaking points made by brunner&lay are 1045. i have some
>broken points in my resource pile. if you're not in a hurry just pick them
>up next time you have a job over this way. otherwise i will ups. i think
>the points i have are about 1-1/4"or 1-1/2" hex.
>
>you might check out the place near you that rents out compressers and
>jackhammers. or call a concrete/road contractor. they probably have some
>broken ones laying around. never know you might pick up some work.
>
>bob