[TheForge] Stone Mason chisels
[email protected]
[email protected]
Mon Mar 18 14:55:10 2002
dave,
the pavement breaking points made by brunner&lay are 1045. i have some broken points in my resource pile. if you're not in a hurry just pick them up next time you have a job over this way. otherwise i will ups. i think the points i have are about 1-1/4"or 1-1/2" hex.
you might check out the place near you that rents out compressers and jackhammers. or call a concrete/road contractor. they probably have some broken ones laying around. never know you might pick up some work.
bob
__________
>I have been asked to make some stone mason chisels. 1 "liner" and 1
>"chipper"(?). I'm pretty sure the one is called a liner (this is the sharp
>one). But I'm not sure of the correct name for the other one, the
>'chipper'. Basically this one looks like the 'liner' but is flat bottomed,
>with a very slight bevel to one side.
>
>Anyway, what steel would be best for this? I'm thinking something in the
>S-? series would be what is needed, but which one? These are hand chisels
>and I'll need to get the stock in hex bars. Definitely a job for the power
>hammer.
>
>
>Dave Brown
>Heritage Smithing
>Green Bay, WI
>ABANA, UMBA, GoM, MODA, ARG
>
>_______________________________________________