>One of my clients wants me to put some blue color in the chain I am making
>for him to match some other material he has. I have tried heating till I
>see the blue color and then quenching in oil, but the color mostly goes away
>by the time the piece cools. What is the secret to getting a real nice blue
>that I have seen on some knives etc, should I be quenching in some magic
>brew or or or?
>
Bake in the oven at the correct temp?