[TheForge] Working copper
[email protected]
[email protected]
Tue Mar 12 15:00:11 2002
Many thanks for the advice on edge joining copper...very much appreciated.
But a question, Dave, and probably a dumb one. What do you mean by 'tinning
the tabs first'? Do you mean just fluxing and putting solder on them or
actually putting tin on them? I do have some pure tin if necessary. I'm kinda
guessing that is just an expression for soldering but I aint got too many
more pieces of copper to screw up and trying to get it near right.
Also another question, if I may: If successfully soldered, should I be able
to cold work them flat just as if it was the copper sheet, without them
coming apart?
Kindest thanks again
Don Plummer