Sat Mar 9 10:15:01 2002
It is a 81 page book, short and to the point. It has metallurgical
information but not text book type.Materials are described by use,
composition,properties and welding procedures. It has a spark test
diagram. It covers ferrous,non-ferrous,tempering and hardening.A good
quick reference book. Bob
----- Original Message -----
From: "Woolley" <[email protected]>
To: <[email protected]>
Sent: Friday, March 08, 2002 9:08 PM
Subject: Re: [TheForge] non-ferrous metals
>
>
> Bob Bergman wrote:
> >
> > Try- Metals for Engineering Craftsmen, BK164 Centaur Forge Catalog.
Bob
> >
>
>
> Bob,
>
> I've considered buying this book in the past. Care to write a brief
> synopsis or review?
>
> cheers,
> Bill Woolley
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
>