Won't work.  Any moisture that gets in will condense on your rods.  Keep =
them warm, not cold. =20
Bruce
NJ

>>> "Shannell" <[email protected]> 03/02/02 07:23PM >>>
What about storing rods in a fridge thats working ie 4 deg C or so. I have =
a
bar fridge in my workshop and thought of using that but never got round to
it, isnt a really cold enviroment extremely dry also, thats all we're =
after
right, keeping things dry?

----- Original Message -----
From: "Dave Brown" <[email protected]>
To: <[email protected]>
Sent: Sunday, March 03, 2002 12:28 AM
Subject: Re: [TheForge] welding rod storage


> At 08:57 03/02/02 -0500, you wrote:
> >never been to green bay ... but i watch the news and if 25 will work in
green
> >bay it damn well outta work here... er ugh... how did you know how =
often
i
> >open the kitchen frig door.... :-)             thanks
>
> I don't.  But I make a small wager that you eat and snack food more =
often
> than you use welding rods.  <grin>
>
> d
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge=20
> theforge mail list group photo site is
> http://www.photoaccess.com=20
> Login:  [email protected]=20
> password:  anvil
> ___________
>
>
>

_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge=20
theforge mail list group photo site is
http://www.photoaccess.com=20
Login:  [email protected]=20
password:  anvil
___________