probably cause the round stock is handy.:)
Phil <[email protected]> wrote: I was looking at the techniques section of WINIKOFF'S KEEN-JUNK PAGE the other day:
http://www.keenjunk.com/_bsj/200205_17-1.htm
There was a page or two from the Blacksmith's Journal about making tong bits from round stock. I have always used square stock, most commonly 3/4" square.
What is the advantage of using round stock? It seems to me that with square stock, it's easier to keep things parallel and perpendicular.
Phil Rosche
Summerville, SC
_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login: [email protected]
password: anvil
___________
---------------------------------
Do You Yahoo!?
Yahoo! Health - Feel better, live better
--- StripMime Report -- processed MIME parts ---
multipart/alternative
text/plain (text body -- kept)
text/html
The reason this message is shown is because the post was in HTML
or had an attachment. Attachments are not allowed.
Please post in Plain-Text only.---