[TheForge] Tapping screw threads question

Ray Miller [email protected]
Wed Jul 24 16:55:08 2002


I use Tap Magic cutting fluid. Almost any cutting fluid for machining 
would work, CimCool, etc.
Ray Miller
Cincinnati

Margaret Green wrote:

>  When tapping screw threads do you use oil? What kind? I haven't
>done this before.
>Thanks. 
>Rich Green
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login:  [email protected]
>password:  anvil