[TheForge] texturing long stock

Gladish Family [email protected]
Mon Jul 15 13:55:01 2002


This one is a pair of garden gates- simple 2 wide x4 tall frames, arched a
bit on top.
I wanted to do upset corners (even though they could easily have been
welded) on the tops, so it made sense to do it in one 12' piece. That is,
until I tried to handle those long sticks in and out of the forge and
hammer!
Next time I'll get help or weld...
Andy G.

> I recently did a gate that was 4' wide and 7' tall.
> The background was basically 6 big scrolls. Each
> scroll required 9' of material. (too long to work with)
> I cut the 9' into three pieces, the cuts were made in a
> place where the scrolls would be touching another
> scroll or the frame so that the weld could be easily
> blended & or collared.
> dave m
>