Did a lot of searching a few years back on quality
blades and the I concur that the best readily
available blades are the Lenox White blade. I use them
for cutting most of my stock and they last forever as
long as you are cutting mild steel or anealed carbon
steel.
FFaller
--- Dan Rathburn <[email protected]> wrote:
> We have a differance of opinion at the farm as to
> when hacksaws where first
> available. Can anyone give me a date and refferance
> to back that
> information?
>
> and
>
> Who is it that makes the best blades for them and
> what retail place can I
> find them?
>
>
> Dan Rathburn
> Elgin, IL USA
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>
=====
Frederick W. Faller
Shiloh Forge Ironware http://users.rcn.com/ffaller/SFI_web.htm
www.immerland.com
__________________________________________________
Do You Yahoo!?
Yahoo! Autos - Get free new car price quotes
http://autos.yahoo.com