Dave Brown wrote:

> Oops, I think you made a little goof.  The S7 is air hardening (see
> abouve), S5 is Oil or Water hardening (see previous post).

	Apparently, but as I recall S5 doesn't water harden well.
	Oil I can believe.  That, or I'm coimpletely senile, which
	is not entirely out of the realm of possibility.