Have fun with the big wedge! Cut the re-bar half way through with a
hacksaw. Then hold the piece over the edge of the anvil or vise and bend
over. If it snaps off and you see crystals, it's steel, if it looks like a
piece of wood breaking its Wrought Iron
L Brown
>NEW TOPIC:
>I have been given some very old ( for AZ. ) re-bar . Someone just tore down
>a useless old historical building, The bar is twisted and varies from .50"
>to 1.50"
>could this be Wrought Iron?
>
>Thank You