[TheForge] fork material
Kenny O'Loughlin
[email protected]
Sat Jul 6 15:31:00 2002
I made a carpet spike to fit on a fork lift, I had to cut the Horizontal =
portion
off to make it work. Now I have this brand new 100# or so wedge . I have =
not=20
found reference to this "FORK " in the machinery's hand book.
NEW TOPIC:
I have been given some very old ( for AZ. ) re-bar . Someone just tore =
down=20
a useless old historical building, The bar is twisted and varies from =
.50" to 1.50"
could this be Wrought Iron?
=20
Thank You