5 minute epoxy is water soluble over time.  Supposedly the longer setting 
stuff (like devcon) is much better.  I don't use devcon, but bet others 
here do<G>.

At 02:51 PM 1/30/2002 +1030, you wrote:
>Im installing a very large door and wanted to support its weight on a pin
>set into concrete, what type of epoxy do i use for this type of application?