The blades will not cut wet, in my experience. Its ends up being a matter of
patience and type of wheel you buy. Try to buy blades less than 1/8" thick.
Thicker blades tend to heat up faster. I have also found the most effective
chop saw blades appear to all grit. Most blades you find out there are
clearly made with fiberglass reinforcement. I believe the blades that do not
have visible fiberglass cut faster and drag less. The do, however wear out
faster. There is no perfect solution other than investing a cold saw. (One
of my some day, one day wish list items).
Ray 
Cincinnati

-----Original Message-----
From: Jeff Harding [mailto:[email protected]]
Sent: Monday, January 28, 2002 9:34 AM
To: [email protected]
Subject: Re: [TheForge] Chop Saw Irritation


This raises a question in my mind... How about a water quench on the
cut?  Not a stream of water, but perhaps a small fine mist directed a
the entry point of the cut?  Are the blades made with adhesive that
will allow this?  What other problems would there be that I'm not
seeing, other than needing to keep it all wiped off and maybe  sprayed
with a water displacer. ( I wouldn't spray the blade)

Jeff   ><>


----- Original Message -----
From: "Miller, Ray (GEAE)" <[email protected]>
To: <[email protected]>
Sent: Monday, January 28, 2002 9:24 AM
Subject: RE: [TheForge] Chop Saw Irritation


> Most likely you have heated up the piece you are cutting so hot it
is
> starting to soften and will not cut worth a damn. Especially if it
is fairly
> thick. Just like the instructions say, let the wheel do the cutting.
If you
> bear down too much it will usually heat up faster and then you're
out of
> luck. You'll have to quench the piece to cut it cleanly.
>
> Ray Miller
> Cincinnati
>
> -----Original Message-----
> From: RW [mailto:[email protected]]
> Sent: Monday, January 28, 2002 9:17 AM
> To: [email protected]
> Subject: [TheForge] Chop Saw Irritation
>
>
> Has anyone noticed that while cutting through a piece of mild steel,
> especially hot-finished, that the sparks are abundant and the wheel
seems to
> be moving right through the piece, then suddenly, the sparks
diminish to a
> small stream and it seems that one has encountered a "hard spot".
Sometimes
> extra pressure seems to get the wheel through this spot but
sometimes
> nothing helps and the wheel just stays there not moving.  The
Instructions
> say, let the wheel do the work.  Do not bear down on the metal.  But
> frequently that does not work.  What is going on here?  What can be
done to
> resume a nice straight and easy cut?
> RW
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>
>

_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  [email protected]
password:  anvil
___________