Humbled RW......... Some day you will come across a DC welder and
be pleasantly surprised at how your welds will start, flow, and look in the
end.
So there's still hope.......
Ralph
----- Original Message -----
From: "RW" <[email protected]>
To: <[email protected]>
Sent: Friday, January 25, 2002 9:23 PM
Subject: Re: [TheForge] welding 1 1/2" square
> I used 6011 in 1/8. Had trouble getting it started but it finally ran for
> me. It is well stuck but it aint purdy. Its been about 20 years since I
> used a stick and never was much good. The welds will be hidden by
fireplace
> ashes. However, I need to hide them from my wife also because I always
> point out shoddy technique and workmanship on ironwork in her decorating
> magazines etc. If she sees my "lovely beads", my aesthetic highground
will
> be lost for a long time.
> RW, the humble
>
> ----- Original Message -----
> From: Ralph Sproul <[email protected]>
> To: <[email protected]>
> Sent: Thursday, January 24, 2002 2:48 PM
> Subject: Re: [TheForge] welding 1 1/2" square
>
>
> > RW, For penetration get some 6011 when using AC. The 6013 and 7014
rods
> > are for deposition and smooth flow. If you want some dig, strength,
fast
> > freeze, with a little rust or dirt - the 6011 is the best. If you want
> to
> > do the least clean up and aren't worried about structural integrity use
> the
> > 6013. I'd also get 1/8 rod for stringer beads if you are going to buy
> > just one size.
> >
> > Ralph
> >
> > ----- Original Message -----
> > From: "RW" <[email protected]>
> > To: <[email protected]>
> > Sent: Thursday, January 24, 2002 11:43 AM
> > Subject: Re: [TheForge] welding 1 1/2" square
> >
> >
> > > Thanks to all. I need to buy some new dry rod. Would you recommend
> 6013
> > > for this application?
> > > RW
> > > ----- Original Message -----
> > > From: Miller, Ray (GEAE) <[email protected]>
> > > To: <[email protected]>
> > > Sent: Thursday, January 24, 2002 9:10 AM
> > > Subject: RE: [TheForge] welding 1 1/2" square
> > >
> > >
> > > > Absolutely!! What you need to do is grind in a "weld Prep". Chamfer
> the
> > > ends
> > > > of each side of the butt joint. When you go to make the weld, not
> > actually
> > > > butt the ends together. Leave a gap, less than an 1/8" and then put
in
> a
> > > > root pass. The gap will improve your chances of good solid root pass
> > > fusion.
> > > > Then put in your cover passes until you have enough material to
grind
> > back
> > > > the surface for finishing. Or if esthetics is secondary, put in a
nice
> > > final
> > > > cover pass and your good to go.
> > > >
> > > > Ray Miller
> > > > Cincinnati, Ohio 4
> > > >
> > > > http://www.casealum.org/alumnuswinter2001/page6.htm
> > > >
> > > > http://www.uc.edu/profiles/rmiller.htm
> > > >
> > > > _______________________________________________
> > > > http://mailman.qth.net/mailman/listinfo/theforge
> > > > theforge mail list group photo site is
> > > > http://www.photoaccess.com
> > > > Login: [email protected]
> > > > password: anvil
> > > >
> > > > -----Original Message-----
> > > > From: RW [mailto:[email protected]]
> > > > Sent: Thursday, January 24, 2002 8:32 AM
> > > > To: [email protected]
> > > > Subject: [TheForge] welding 1 1/2" square
> > > >
> > > >
> > > > Is it possible to butt weld 1 1/2" solid mild steel with a 230 amp
> max.,
> > > AC
> > > > 220v welder?
> > > > It does not need to be a "structural weld", just to hold a fireplace
> > grate
> > > > frame together.
> > > > I tried it with a #7 oxy/acet tip which is for 1 1/4" max and it is
> not
> > > much
> > > > better than if I had used chewing gum.
> > > > RW
> > > >
> > > >
> > > > _______________________________________________
> > > > http://mailman.qth.net/mailman/listinfo/theforge
> > > > theforge mail list group photo site is
> > > > http://www.photoaccess.com
> > > > Login: [email protected]
> > > > password: anvil
> > > > ___________
> > > >
> > > > _______________________________________________
> > > > http://mailman.qth.net/mailman/listinfo/theforge
> > > > theforge mail list group photo site is
> > > > http://www.photoaccess.com
> > > > Login: [email protected]
> > > > password: anvil
> > > > ___________
> > > >
> > > >
> > > >
> > >
> > > _______________________________________________
> > > http://mailman.qth.net/mailman/listinfo/theforge
> > > theforge mail list group photo site is
> > > http://www.photoaccess.com
> > > Login: [email protected]
> > > password: anvil
> > > ___________
> > >
> > >
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: [email protected]
> > password: anvil
> > ___________
> >
> >
> >
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>