[TheForge] Trenton Anvils

Peter Fels and Phoebe Palmer [email protected]
Sun Jan 20 01:59:00 2002


At 09:01 PM 1/19/02, you wrote:

Trentons are fine anvils...PF


>If I remember the "Anvils in America" book correctly, the top half is forged
>and the bases are cast. That's why many break there.
>
>On my Trenton, the weight is readable on the foot, facing the front, under
>the horn, on the left side as you have the horn pointing at you. The number
>on the right side, usually starting with an A, is the serial number.
>
>Ray Baker
>Frontier Forge
>Olympia, WA
>
>----- Original Message -----
>From: Woolley <[email protected]>
>To: <[email protected]>
>Sent: Saturday, January 19, 2002 7:59 PM
>Subject: [TheForge] Trenton Anvils
>
>
> >
> >
> > Greetings,
> >
> > Does anyone use a Trenton anvil?  Are they forged or cast?  How are they
> > marked?  I was offered a 100 lb. but seller wasn't positive about the
> > weight.  I didn't see it.  Worth pursuing?
> >
> > Regards,
> > Bill Woolley
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login:  [email protected]
> > password:  anvil
> > ___________
> >
> >
>
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://www.photoaccess.com
>Login:  [email protected]
>password:  anvil
>___________