[TheForge] Cheap clear finish question

Chris Worsley [email protected]
Mon Jan 14 07:26:00 2002


Hi Bob,
I used Watco oil a few times years ago and found that it turned gummy on the piece after time. I applied it to work that was warm enough to make it flow
easily into all crevices, and buffed when cool and "dry". Since then I have used the beeswax/boiled linseed oil/terps mix and found it better. (indoor work
only)

Chris
Alexandria VA

[email protected] wrote:

> i've never used it but have heard that watco (used by a lot of woodworkers) makes a decent finish for metal. has anyone tried watco or have any comments.
>
> bob s.