[TheForge] Cheap clear finish question
Steve Smith
[email protected]
Sat Jan 12 17:20:49 2002
Wax works great.
Steve Smith
Barking Crow wrote:
> Hey,
>
> My daughter is refinishing a couple of metal chairs and table and I've
> helped her wire brush the old paint off and convinced her that the beauty of
> the bare steel is much greater than that of paint and want to help her spray
> paint a clear finish on them. Short of going the powder coat route I'm
> wondering what the best cheap easy (get my drift?) route is? I'm torn
> between lacquer from a spray can or polyurethane from a spray can. The
> chairs and table are for inside use. Opinions?
>
> Thanks, Jeff Valentine
>
> Barking Crow
> http://www.barkingcrow.com