> Turpentine and heat. > > Darrell Thanks, Darrell, I'll try it. It needs to stay liquid at about 75 degrees, at least for as long as it takes to apply it. I know a mixture of the waxes, warmed and mixed with turpentine and linseed oil will work, but the linseed oil stinks for a month or more- no good for inside the house! Andy G.