Yeah I found that with the ball valve too, now its off or on. My tips
probably do last longer than 20mins mabey more like 40, then the hole is
twice the diameter it started with and air flow goes up dramatically and the
compressors have trouble keeping up.

----- Original Message -----
From: "marc" <[email protected]>
To: <[email protected]>
Sent: 09 December, 2002 6:20 PM
Subject: Re: [TheForge] Sandblasting nozzles


> Is he talking about the ceramic tip or the ball valve?
> I went through my first ball valve in 20 minutes. It seems if you try to
> adjust the flow with the final ball valve it will eat the ball inside very
> quickly. I learned all the way on or all the way off. Adjust the air flow
> not the final valve where the sand comes out.
> ----- Original Message -----
> From: "Walter L. Mullett" <[email protected]>
> To: <[email protected]>
> Sent: Monday, December 09, 2002 8:47 PM
> Subject: Re: [TheForge] Sandblasting nozzles
>
>
> > Shannell,
> >
> > I used to do a lot of work with a monument shop that engraved granite
with
> a
> > sandblast unit.  Their ceramic tips would last for months with almost
all
> > day, every workday use.  Something must be wrong with your setup.
> >
> > Walt
> > -----Original Message-----
> > From: Shannell Sugrue <[email protected]>
> > To: [email protected] <[email protected]>
> > Date: Monday, December 09, 2002 8:31 PM
> > Subject: [TheForge] Sandblasting nozzles
> >
> >
> > >Enquired today about some replacement ceramic nozzles for my chinese
> > >pressure pot  sandblaster, they are $10 ea and last about 20-30 mins,
rip
> > >off if you ask me, Ive heard of using tungsten nozzles, are these more
> > >economical, can tungsten be machined on a lathe so I could make my
own??
> or
> > >can I use some other type of metal and lathe/drill them up?
> > >
> > >_______________________________________________
> > >http://mailman.qth.net/mailman/listinfo/theforge
> > >theforge mail list group photo site is
> > >http://www.photoaccess.com
> > >Login:  [email protected]
> > >password:  anvil
> > >___________
> > >
> > >
> > >
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login:  [email protected]
> > password:  anvil
> > ___________
> >
> >
> >
>
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
>
>