Ditch the regulator that you have and get a "high volume/pressure" one from
your propane company.
dave m

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of jacques gallant
Sent: Tuesday, August 27, 2002 5:13 PM
To: [email protected]
Subject: [TheForge] propane forge




I built a propane forge according to the plans by Hans Peot
(http://www.abana.org/downloads/education/pipeforge.pdf) and i am having
some trouble getting it up to heat.  Well the "flame holder" gets up to a
very pretty orange (not quite yellow, but above cherry red) and the whole
body gets almost too hot to touch in a few minutes, but it doesn't seem to
do much to heat metal-not like my coal forge.

The pressure for my propane is being controlled by an acetylene regulator,
and the blower provides at least 150 cfm, but I can't seem to get the whole
inside of the forge to fill with that pretty orange flame that i've seen in
other people's forges.  I must confess, i made one slight modification to
the design, i used 12 inch pipe instead of 10 inch pipe for the body of the
forge because I wanted something slightly more all purpose than a small
bladesmith's forge.

If anyone has any ideas on the matter, i'd appreciate them, i've been having
a hard time finding anyone who knows anything about propane.

_________________________________________________________________
MSN Photos is the easiest way to share and print your photos:
http://photos.msn.com/support/worldwide.aspx

_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://www.photoaccess.com
Login:  [email protected]
password:  anvil
___________