[TheForge] Re: Pure Iron
[email protected]
[email protected]
Fri Aug 2 21:55:01 2002
Well, I can't answer for anyone else, but in my case, while I would have
liked to try it, I could not justify the minimum order plus shipping.
Several attempts to combine orders with other interested parties just never
happened. Add to that, the size I use most frequently (3/8" square) rarely
seemed to be in stock. With a lower minimum, you'd have gotten my business.
Jerry V
Williamsburg, VA
<< We remain puzzled
as to why Pure Iron use has grown so well in Europe and so poorly here as
the
cost ratio between low carbon and Pure Iron in Europe is about ten times,
where here it may be around 2 to 2-1/2 times the cost of low carbon. >>