Andy, the tarnished pipe against the newly soldered in fittings
looks pretty tacky at the moment. :-(
Ralph
----- Original Message -----
From: "Andrew Vida" <[email protected]>
To: <[email protected]>
Sent: Tuesday, April 30, 2002 10:06 AM
Subject: Re: [TheForge] copper arch
> Why not leave it on. Nature's been working very hard on it for all
> that time. Just a thought.
>
> Otherwise, HCl seems to work nicely, but be careful.
>
> Ralph Sproul wrote:
> >
> > Any suggestions for cleaning up 50 feet of copper tubing for an
arch
> > (15 year tarnish on it).
> >
> > Ralph
> >
> > _______________________________________________
> > http://mailman.qth.net/mailman/listinfo/theforge
> > theforge mail list group photo site is
> > http://www.photoaccess.com
> > Login: [email protected]
> > password: anvil
> > ___________
>
> --
> -Andy V.
>
> At the end of the day, all we really own is our breath.
>
> Quite an experience living in fear, isn't it?
> That's what it means to be a slave.
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login: [email protected]
> password: anvil
> ___________
>
>