At 08:44 AM 4/16/2002 -0400, you wrote:
>Hey,
>
>How do you keep it from work hardening? Thanks, Jeff Valentine
Well, if you don't keep a steady push on the drill bit, the bit will just
polish the surface and work harden it nicely. So, keep a steady push on
the drill bit so that you are always cutting a bit of new copper. Make
sense?