[TheForge] Rose pedal patterns

Larry [email protected]
Tue Apr 9 12:06:01 2002


That's the ticket!  There just happens to be one of those silk roses right here
on my book shelf!  Thanks, I'm in business.

Larry

"Dick M. Snow" wrote:

>
> Go to the local Walmart or such and buy a fake silk rose. Take it back to
> the shop and take it apart. Iron the pieces out flat and trace away.
>
> Dick M. Snow ([email protected])