[TheForge] ITC-100

Jay Hayes [email protected]
Fri Apr 5 18:34:01 2002


Geoff,

I am also a distributor for ITC-100, and also carry a complete line of supplies
for building gas forges, as well as several gas forge kits and burner kits.

Jay Hayes
C. J. Products Inc.
 [email protected]


"Daniel T. Hayes" wrote:

> Geoff:
>
> Try this link: http://www.budgetcastingsupply.com/ITC.html
>
> ----------------------------------------------------------------------------
> ----
> Description:
> ITC-100 HT Ceramic Coating is a versatile high temperature coating that has
> proven to achieve outstanding energy savings and refractory protection.  Use
> it alone or as a base coat for other ITC products.  It is used as a covering
> for ceramic fiber insulation or castable refractory. This material reflects
> radiant heat back into the furnace to achieve high temperatures quickly and
> efficiently.
> ----------------------------------------------------------------------------
> ----
> How To Use It:
> ITC-100 HT Ceramic Coating:  Preparation: Prepare the surface by removing
> all loose and weakened fiber, bricks, debris, particles, dust and grease
> from interior walls, door, crown, floor and grooves behind electrical
> elements.  Immediately before applying ITC 100, dampen these areas by
> spraying lightly with water. Mixing: Mix to one pint of ITC 100 1/2 pint of
> water and mix well.  Applying: Spraying is the best method of application.
> For small applications a brush can be used.
>
> WARNING:  Do NOT apply any surface coatings, such as ITC-100 or ceramic
> fiber blankets over refractory cement until the refractory is fully calcined
> (cured and fired).  Sealing the surface has caused steam explosions as the
> refractory heats!!
> ----------------------------------------------------------------------------
> ----
>
> Another link is: http://www.wardburner.com/itc.cfm. A good search engine
> should give you quite a few hits, many are in German. The price appears to
> be around $25/pint, $80/half-gallon and $140/gallon with coverage being
> 50-75 square feet per gallon.
>
> Hope this helps,
> Dan
>
> -----Original Message-----
> From: [email protected]
> [mailto:[email protected]]On Behalf Of [email protected]
> Sent: Friday, April 05, 2002 4:39 PM
> To: [email protected]
> Subject: [TheForge] ITC-100
>
> What is this stuff, who makes it and so on? I asked the rep from our
> local Kaowool agents, and they knew nothing about it.
>  Does it go under other names?
> Geoff
> (New Zealand)
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________
>
> _______________________________________________
> http://mailman.qth.net/mailman/listinfo/theforge
> theforge mail list group photo site is
> http://www.photoaccess.com
> Login:  [email protected]
> password:  anvil
> ___________