The angle depends on what you are using it for. The big ones that are used 
to cut r.r. rail are at 40 to 45 degrees,slitting at about 20 to25 degrees. 
For most general use tools I like to radius the grind to the edge (stays 
sharper longer and doesn't deform as fast.)