[TheForge] cleaning up aluminum for welding
Dan Tull
[email protected]
Thu Dec 20 21:52:49 2001
Xylol, xylene, acetone.
On Thu, 20 Dec 2001 14:47:28 -0500 evelyn hart <[email protected]>
writes:
> What is the best way or method for cleaning up aluminum before
> welding,
> especially cast aluminum with cracks? I am talking about oil, grease
> and
> etc. that could get down in the crack.
>
> Bobby Hart