[TheForge] heating copper in a forge (yak)

P. McComb [email protected]
Sat Dec 15 10:23:00 2001


Copper Pennies???  Must be really old then...8^)


Paul McCombPaul McComb
Fat Raccoon Forge
[email protected]

-----Original Message-----
From: [email protected]
[mailto:[email protected]]On Behalf Of Herman, Richard A
Sent: Friday, December 14, 2001 5:13 PM
To: '[email protected]'
Subject: RE: [TheForge] heating copper in a forge


Rumor I heard once was that if you wanted to have fun with someone getting
ready to forge weld, all you had to do was to throw a penny into the fire.
Somehow the copper in the penny was supposed to keep a forge weld from
working.  Don't know why, could just be an old wives tale.  I think the
problem was corrected by tearing the fire apart and starting fresh.

Rich Herman

-----Original Message-----
From: [email protected] [mailto:[email protected]]
Sent: Friday, December 14, 2001 3:55 PM
To: [email protected]
Subject: [TheForge] heating copper in a forge


somewhere i heard that you shouldnt heat copper or other metals in the same
forge as steel ... is there a difference between a coal or propane forge ...

i hammer a little steel but also work with copper ... any ideas.... thanks
_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://albums.photopoint.com/j/AlbumList?u=1169182
___________

_______________________________________________
http://mailman.qth.net/mailman/listinfo/theforge
theforge mail list group photo site is
http://albums.photopoint.com/j/AlbumList?u=1169182
___________