Define divot....
If its just a dent grind it out, if its a chink, I'd work around it. If its
a chunk, then look at fixing it.
At 11:06 PM 5/14/01 -0500, you wrote:
>Hey all,
> I know this has been discussed but i didn't pay attention and now I
>need the advice. I have a divot in my anvil. Can I use my lincoln stick
>welder to fill it and then smooth it with the grinder? Will it be too
>brittle? Will I screw up the anvil? Should I just continue to live with
>it?
>
>Dan
>www.visi.com/~irontree
>--
>"Isn't sanity just a one-trick pony anyway? I mean, all
>you get is that one trick, rational thinking, but when
>you're good and crazy, well, the sky's the limit!"
>
> - The Tick
>_______________________________________________
>http://mailman.qth.net/mailman/listinfo/theforge
>theforge mail list group photo site is
>http://albums.photopoint.com/j/AlbumList?u=1169182
>___________
Michael Linn
Artist Blacksmith
McCalla, Alabama
AFC Webmaster
http://afc.abana-chapter.com