My solderwick is pre-fluxed (try saying that fast!).
On 30/8/07 21:19, "elecraft-request at mailman.qth.net"
<elecraft-request at mailman.qth.net> sent:
> I've found that putting some flux on the solderwick braid helps
> tremendously in drawing out the solder on the pads and in the holes
> without overheating them.
>
> I take a new roll of solderwick, pull out about 2 feet of braid, and
> apply liquid soldering flux to it and let it soak in overnight. Then
> I roll it back onto the spool, and I'm ready for the next repair.
>
> 73,
> ed - k9ew
> www.k9ew.us
--
Now, here, you see, it takes all the running you can do, to keep in the
same place. If you want to get somewhere else, you must run at least twice
as fast as that! -Lewis Carroll, mathematician and writer (1832-1898)