The original bridge would have definitely been wrought, when they re did it anything changed would not be. Comment say that a road crew attached a cable to the tree for some reason and as the bridge failed it pulled the tree down(tree looks dead).. Driver should get new underwear and pants!
Have a battery powered sawsall? I wonder if they finished inspecting it?
Larry

> On Oct 26, 2025, at 1:59 PM, Bruce <freemab222 at gmail.com> wrote:
> 
> https://www.youtube.com/watch?v=7E1MUxI3nlk
> 
> Looks like a riveted construction.  Whaddaya wanna bet it's wrought iron?
> Anyone care to salvage it?  I doubt it will be renovated again, more likely
> replaced with some pre-fab.
> 
> Bruce
> NJ
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
> 
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
> 
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> Message delivered to lp.brown at verizon.net



More information about the TheForge mailing list