The best method I have seen is a bead cheater.. the ratchet strap can
work, but it's hit or miss.. sometimes it just forces the bead in more..
I have 2 QC's for my air hose.. I put on a full flow tire inflator and have
a safety air gun on the other as I inject air into the valve stem, I also
shoot air from the air gun into the bead being sure to keep the air gun
from to close to the tire/bead/rim combo.. And there you have it..
I also use a tire safe wax to help lube the tire and rim and it also helps
to seat the bead at a lower pressure.. Its both steel and alumimun safe..
JLP Services Inc
6 Kenwood Dr
Rutland, MA 01543-1215
1 (508) 667-5498
On Sat, Mar 30, 2019 at 10:03 AM Kim George <klgeorge at kent.edu> wrote:
> If you have a small ratcheting cargo strap put it around the tire and
> tighten it.It will push the beads of the tire to the rim. Just
> remember to remove before trying fill the tire completely.
>
> --
> Kim George
>
> "Why for you try to bury me in cold,cold ground?"
> Taz
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
>
More information about the TheForge
mailing list