We have beat this one to death, but one more swing with a club.
If the forge is going to sit outside - rain and moisture all the time, clay
may not be the best thing. The coal runoff will be sulfuric acid and may
well eat up your forge.
I put straps on my old forge to hold it together. The expansion sheared
the 1/4/20 bolts. I ended up getting some nickel rod and welded up the
crack.