I'd hate to fill that quench tank, I hate paying for the couple of gallons of oil I use.
Charles.

      From: Dave Smucker <davesmucker at hotmail.com>
 To: Charles <xlch58 at swbell.net>; Blacksmithing List Sponsored by ABANA <theforge at mailman.qth.net> 
 Sent: Sunday, July 30, 2017 8:14 PM
 Subject: RE: [TheForge] An Impressive Quench
   
Very interesting photo.
Based on your time frame this would have been a Leopard tank.  The industrial building, cranes and heat-treat furnace look like they are from this time frame (70's) as you noted and not WWII time frame.
I have never seen large complex castings of this type heat-treated but have seen large rolls oil quenched.  Oil is the quench medium of choice for such a complex shapes as water would likely result in very serious distortion and cracking failures.  The oil used would be special industrial quench oil.

Dave Smucker
Brasstown, NC



-----Original Message-----
From: theforge-bounces at mailman.qth.net [mailto:theforge-bounces at mailman.qth.net] On Behalf Of Charles
Sent: Sunday, July 30, 2017 8:36 PM
To: Blacksmithing List Sponsored By ABANA
Subject: [TheForge] An Impressive Quench

This is an image of a Panzer tank hull being quenched in the 60s or 70s.   I stopped using crankcase oil and now use olive oil since it smells better.  No matter what oil they use there, that has got to reek. https://s3-us-west-1.amazonaws.com/hmt-forum/tank_quenching.jpg


Charles
______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net

TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil

This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html Message delivered to davesmucker at hotmail.com


   


More information about the TheForge mailing list