[TheForge] Titanium pins
Dave Mudge
davemudge1 at gmail.com
Mon Jan 9 13:19:51 EST 2017
I wonder if silver solder or 'sil-fos' would work to join the ends.
I think that the medics will give up the pins after running through the
autoclave...
thanks, this is good.
keep going,
dave m
your list mom
On Mon, Jan 9, 2017 at 11:23 AM, Charles <xlch58 at swbell.net> wrote:
> The biggest issue is getting them to give you the pins. Often they treat
> them as medical waste and will not let you near them. Depends on the Dr.
>
> Charles
>
> > On Jan 9, 2017, at 8:59 AM, davemudge1 <davemudge1 at gmail.com> wrote:
> >
> >
> >
> > Thanks for the input Mike. They will remove the pins soon because he is
> still growing and the bones are mending well.
> >
> >
> > Sent via the Samsung Galaxy Note® 4, an AT&T 4G LTE smartphone
> >
> > -------- Original message --------
> > From: mspencer at tallships.ca
> > Date: 1/9/2017 1:26 AM (GMT-06:00)
> > To: theforge at mailman.qth.net
> > Subject: [TheForge] Titanium pins
> >
> >
> >> My 13 year old grandson broke his arm a short time ago and had 2
> >> pins put into the bones to hold them together. from the x-rays they
> >> appear to be 3/16 diameter and as long as from his wrist to his
> >> elbow....twisted wire bracelet with those pins when they are
> >> removed.
> >
> > Has anyone said that they'll ever be coming out? I broke my right
> > elbow in a hockey game circa 1958, fixed up with a steel pin and it's
> > still there. Nice work: it's never caused me any trouble with
> > swinging a hammer.
> >
> > No help on the titanium, though, sorry. The only surgical implant I
> > ever had in the shop was a metal prosthetic hip joint. It was so
> > pretty that I didn't want to do anything to alter it, made banded
> > attachments to convert it to a door knocker.
> >
> > Oh, and best regards to your grandson. It can't have been a fun
> > holiday experience.
> >
> > - Mike
> >
> > --
> > Michael Spencer Nova Scotia, Canada .~.
> > /V\
> > mspencer at tallships.ca /( )\
> > http://home.tallships.ca/mspencer/ ^^-^^
> >
> > ______________________________________________________________
> > TheForge mailing list
> > Home: http://mailman.qth.net/mailman/listinfo/theforge
> > Help: http://mailman.qth.net/mmfaq.htm
> > Post: mailto:TheForge at mailman.qth.net
> >
> > TheForge mail list group photo site is
> > http://www.shutterfly.com
> > Login: blacksmithblacksmith at hotmail.com
> > Password: anvil
> >
> > This list hosted by: http://www.qsl.net
> > Please help support this email list: http://www.qsl.net/donate.html
> > Message delivered to davemudge1 at gmail.com
> > ______________________________________________________________
> > TheForge mailing list
> > Home: http://mailman.qth.net/mailman/listinfo/theforge
> > Help: http://mailman.qth.net/mmfaq.htm
> > Post: mailto:TheForge at mailman.qth.net
> >
> > TheForge mail list group photo site is
> > http://www.shutterfly.com
> > Login: blacksmithblacksmith at hotmail.com
> > Password: anvil
> >
> > This list hosted by: http://www.qsl.net
> > Please help support this email list: http://www.qsl.net/donate.html
> > Message delivered to xlch58 at swbell.net
>
> ______________________________________________________________
> TheForge mailing list
> Home: http://mailman.qth.net/mailman/listinfo/theforge
> Help: http://mailman.qth.net/mmfaq.htm
> Post: mailto:TheForge at mailman.qth.net
>
> TheForge mail list group photo site is
> http://www.shutterfly.com
> Login: blacksmithblacksmith at hotmail.com
> Password: anvil
>
> This list hosted by: http://www.qsl.net
> Please help support this email list: http://www.qsl.net/donate.html
> Message delivered to davemudge1 at gmail.com
>
--
...sometimes you're the windshield,
...sometimes you're the bug
More information about the TheForge
mailing list