[TheForge] Old band saw blade

Ron Childers ron at munlaw.net
Mon Aug 14 10:42:10 EDT 2017


Thanks, L-6, even if it has carbide teeth brazed onto it? 

-----Original Message-----
From: theforge-bounces at mailman.qth.net [mailto:theforge-bounces at mailman.qth.net] On Behalf Of J. Petrila
Sent: Monday, August 14, 2017 10:37 AM
To: Blacksmithing List Sponsored by ABANA <theforge at mailman.qth.net>
Subject: Re: [TheForge] Old band saw blade

15n20 usually for high speed m42 blades. I believe wood mizer are 15n20 also.

L6 for circular.

You can test by seeing if a test strip will air harden..



On Aug 14, 2017 6:11 AM, "Ron Childers" <ron at munlaw.net> wrote:

I have a piece of old band saw blade without carbide teeth, probably from a Wood Miser. What kind of steel is it likely to be? 15N20 maybe? What steel is used in circular saw blade that has carbide teeth? Thanks, Ron ______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net

TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil

This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html Message delivered to jlpservicesinc at gmail.com ______________________________________________________________
TheForge mailing list
Home: http://mailman.qth.net/mailman/listinfo/theforge
Help: http://mailman.qth.net/mmfaq.htm
Post: mailto:TheForge at mailman.qth.net

TheForge mail list group photo site is
http://www.shutterfly.com
Login: blacksmithblacksmith at hotmail.com
Password: anvil

This list hosted by: http://www.qsl.net
Please help support this email list: http://www.qsl.net/donate.html Message delivered to ron at munlaw.net


More information about the TheForge mailing list